Our merchandise are commonly recognized and reliable by customers and can meet constantly developing economic and social desires for Bh Series Low Voltage Current Transformer, High Permeability Material, 1k107 Strip, We are keeping durable small business relationships with additional than 200 wholesalers in the USA, the UK, Germany and Canada. For anyone who is intrigued in any of our products, make sure you experience free to speak to us.
Special Price for Lcd With Backlight - Fe-Based 1K101 Amorphous Ribbon – Malio Detail:

Description

Product Name Fe-Based 1K101 Amorphous Ribbon
P/N MLAR-2131
Width 5-80mm
Thickness 25-35μm
Saturation magnetic induction 1.56  Bs (T)
Coercivity  2.4  Hc (A/m)
Resistivity 1.30 (μΩ·m )
Magnetostriction coefficient 27 λs (ppm)
Curie temperature 410  Tc (℃)
Crystallization temperature 535  Tx (℃)
Density 7.18 ρ (g/cm3)
Hardness 960  Hv (kg/mm2)
Thermal expansion coefficient 7.6  (ppm/℃)

Application

● Mid-frequency power transformer core, distribution transformer core

● Toroidal uncut cores for smooth filtered output inductors and differential mode input inductors for switching power supplies

● Noise suppression in car stereos, toroidal uncut cores for car navigation system chokes

● Ring-cut cores for PFC power factor correction in air conditioning and plasma TVs

● High frequency rectangular cut cores for output inductors and transformers for switching power supplies, uninterruptible power supplies, etc.

● Toroidal, uncut cores for IGBTs, MOSFETs and GTOs pulse transformers

● High power density variable speed motors, stators and rotors for generators

Features

● Highest saturation magnetic induction among amorphous alloys-reduce components size

● Low coercivity- Improve components efficiency

● Variable Magnetic flux rate – By different core heat treatment processes to meet the requirements of different applications

● Good temperature stability- Can work at -55°C -130°C for long periods of time

● Cores used in transformers are 75% more energy efficient than S9 silicon steel cores in terms of no-load losses and 25% more energy °C efficient in terms of load losses

● Short strip production process and low production cost (see Fig. 1.1)

● The strip has a special microstructure which determines its excellent magnetic properties (Fig. 1.2) and performance stability.

● The composition and process parameters of the strip can be quickly adjusted to meet different usage requirements.

● For new energy solar grid-connected inverters

1

Figure 1.1 Amorphous ribbon production process

2

Figure 1.2 Bs versus Hc of different soft magnetic materials

Material comparison

Performance Comparison of Fe-based amorphous alloys with cold-rolled silicon steel

Basic parameters

Fe-based amorphous alloys

Cold-rolled silicon steel(0.2mm)
Saturation magnetic induction Bs (T)

1.56

2.03

Coercivity Hc (A/m) 2.4   25
Core losses(P400HZ/1.0T)(W/kg) 2 7.5
Core losses(P1000HZ/1.0T)(W/kg) 5 25
Core losses(P5000HZ/0.6T)(W/kg) 20 >150
Core losses(P10000HZ/0.3T)(W/kg) 20 >100
Maximum magnetic permeability (μm 45X104 4X104
Resistivity (mW-cm) 130 47
Curie temperature(℃) 400 740

1
2
3
440
5
6
7
11


Product detail pictures:

Special Price for Lcd With Backlight - Fe-Based 1K101 Amorphous Ribbon – Malio detail pictures

Special Price for Lcd With Backlight - Fe-Based 1K101 Amorphous Ribbon – Malio detail pictures

Special Price for Lcd With Backlight - Fe-Based 1K101 Amorphous Ribbon – Malio detail pictures

Special Price for Lcd With Backlight - Fe-Based 1K101 Amorphous Ribbon – Malio detail pictures

Special Price for Lcd With Backlight - Fe-Based 1K101 Amorphous Ribbon – Malio detail pictures


Related Product Guide:

With a positive and progressive attitude to customer's curiosity, our organization repeatedly improves our products top quality to meet the wants of consumers and further focuses on safety, reliability, environmental necessities, and innovation of Special Price for Lcd With Backlight - Fe-Based 1K101 Amorphous Ribbon – Malio , The product will supply to all over the world, such as: Kuwait, Montpellier, Munich, We also have good cooperation relationships with many good manufacturers so that we can provide almost all of auto parts and after-sales service with high quality standard,lower price level and warmly service to meet demands of customers from different fields and different area.
  • After the signing of the contract, we received satisfactory goods in a short term, this is a commendable manufacturer.
    5 Stars By Stephanie from Argentina - 2017.09.26 12:12
    The after-sale warranty service is timely and thoughtful, encounter problems can be resolved very quickly, we feel reliable and secure.
    5 Stars By Iris from Uruguay - 2017.02.14 13:19
    Write your message here and send it to us