inoa mea kūʻai 1K107 Nanocrystalline Ribbon ma muli o Fe
P/N MLNR-2132
Width 5-65mm
Thickness 26-34μm
Saturation hoʻokomo magnetic 1.25 Bs (T)
ʻO ka hoʻokoe ʻana  1.5 Hc (A/m)
Kū'ē 1.20 (μΩ·m )
Mākēneki coefficient 1 λs (ppm)
Ka wela Curie 570 Tc (℃)
Mahana crystallization 500 Tx (℃)
ʻO ka mānoanoa 7.2 ρ (g/cm3)
ʻoʻoleʻa 880
Koefficient hoʻonui wela 7.6

Palapala noi

● Hoʻololi i nā mea hoʻololi mana a me nā core transformer pulse

● Nā mea hoʻololi mana, nā core transformer o kēia manawa

● Leakage pale hoololi transformer hao kumu

● kānana inductors, ikehu mālama inductors, reactor cores

● EMC keʻano maʻamau a me ke ʻano ʻokoʻa inductor core

● ʻO nā mea hoʻoheheʻe Saturation, nā mea hoʻonui mākēneki, nā core suppressor spike a me nā peʻa magnetic

Nā hiʻohiʻona

ʻOi aku ka maikaʻi o nā mea Nanocrystalline Fe-based ma mua o nā mea maʻamau a ʻo ia ka hopena maikaʻi loa no kāu noi (Figure 1.1).

3

Kiʻi 1.1 μr kūʻē i nā Bs o nā mea ʻenekini palupalu palupalu

● High saturation magnetic induction (1.25 T) a me ke kiʻekiʻe magnetic permeability (>80,000) no nā puke liʻiliʻi a me ka pololei kiʻekiʻe

● ʻO ka poho kumu e like me ka 1/5 o ka hao-amorphous, me nā poho ma lalo o 70 W/kg ma 100 kHZ, 300 mT

● Saturation magnetostriction coefficient kokoke i 0, me ka haʻahaʻa haʻahaʻa hana

● Paʻa wela maikaʻi, <10% hoʻololi i nā waiwai waiwai ma luna o ka pae wela -50 a 120 °C

● ʻO nā hiʻohiʻona alapine maikaʻi me ka permeability maikaʻi loa a me nā poho haʻahaʻa ma kahi ākea ākea

● Me ka adjustable magnetic properties, hiki ke loaʻa nā ʻano mea like ʻole ma ka hoʻohana ʻana i nā ʻano like ʻole transverse a me ka vertical field magnetic, a i ʻole me ka mālama ʻole ʻana i ka wela, e like me ka remanence haʻahaʻa, ratio rectangular kiʻekiʻe, a me ka permeability kiʻekiʻe.

Hoʻohālikelike waiwai

Ka Hoʻohālikelike Hana o Fe-based Nanocrystalline Ribbon me Ferrite Core

Nā palena kumu

Lipine Nanocrystalline

Ferrite Core
Hoʻokomo mākia hoʻokahi Bs (T)

1.25

0.5

ʻO ke koena o ka hoʻoulu manaʻo Br (T)(20KHz) <0.2 0.2
Nā poho kumu (20KHz/0.2T)(W/kg) <3.4 7.5
Nā poho kumu (20KHz/0.5T)(W/kg) <35 ʻAʻole hiki ke hoʻohana
Nā poho kumu (50KHz/0.3T)(W/kg) <40 ʻAʻole hiki ke hoʻohana
ʻO ka hoʻokuʻu ʻana i ke kino (20KHz) (Gs/Oe) >20000 2000
Ka ikaika ikaika Hc (A/m) <2.0 6
Kū'ē (mW-cm) <2 4
Koefficient magnetostriction saturated(X10-6 400 740
Palekana (mW-cm) 80 106
Ka Mahana Curie >0.7 -